Electrospinning of poly(ethylene-co-vinyl alcohol) fibers
2019/11/27 21:33:45 admin
Solutions of poly(ethylene-co-vinyl alcohol) or EVOH, ranging in composition from 56 to 71 wt% vinyl alcohol, can be readily electrospun at room temperature from solutions in 70% 2-propanol/water (rubbing alcohol). The solutions are prepared at 80degreesC and allowed to cool to room temperature. Interestingly, the solutions are not stable at room temperature and eventually the polymer precipitates after several hours. However, prior to precipitation, electrospinning is extensive and rapid, allowing coverage of fibers on various substrates, including a grounded metal plate, dielectrics interposed between the charged jet and the metal ground, and on the human body. Fiber diameters of ca. 0.2-8.0 mum were obtained depending upon the solution concentration, an attractive range for tissue engineering, wound healing, and related applications. Electrospun EVOH mats have been shown to support the culturing of smooth muscle cells and fibroblasts. (C) 2002 Elsevier Science Ltd. All rights reserved.
相关推荐
暂无相关推荐
网友评论 请遵循相关法律法规,理性发言
回复
查看更多回复

分享